Customization: | Available |
---|---|
Alloy or Not: | Alloy |
Standard: | ISO9001 |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Application:
It is widely applicable to new type of advanced material and special alloysManufacturing process:
Main products of the chemical composition:
Name | Usage% | Temperature/ºC | Use |
Coverer CHT-FG | 0.8-0.1kg/m2 | <660ºC | All other kinds of aluminium and aluminium alloy except high magnesium alloy. |
Magnesium coverer CHT-MF | 0.5-1.0kg/m2 | 450ºC | Mainly for the covering of magnesium and magnesium alloy to avoid oxidation damage |
Sodium -free coverer CHT-WNF | 0.3kg/m2 | 700-740ºC | For the covering of aluminium melt that cannot touch sodium to avoid oxidizing and damaging the aluminium liquid. |
Fluxer 1 CHT-JL1 | 0.3<0.5% | 640ºC | Used for refining of series of processing aluminium alloy and pure aluminium except for high magnesium and popularly. |
Magnesium Refiner CHT-MJ | 1-1.5kg/Tm | 450ºC | Mainly for the degassing and slag removal of magnesium and magnesium alloy |
Degassing refiner CHT-CJL | 0.1-0.2% | 680-750ºC | Degassing refiner is a relatively traditional lump refiner; it has a double effect of slag removal and degassing. By far, it is widely acknowledged as the most effective solid refiner. |
High-efficiency and Non-toxic Refiner CHT-GJL | 0.1-0.2% | 680ºC | For aluminium and aluminium alloy except high magnesium ally |
Sodium-free Refiner CHT-WNJ | 2-5 kg/T al | 700-730ºC | The product mainly for the aluminium alloy, degassing and slag removal of wheel hubs, pistons and sodium of cars. |
Power spraying refiner CHT-PJL | 0.1-0.2% | 700-750ºC | It has the product mainly |
Universal Fluxer CHT-WN | 0.2-0.5% | 710-750ºC | |
Phosphorus-copper Modifier CHT-LT | 0.4-0.6% | ||
Aluminium-phosphorus Alloy Modifier CHT-LL | 0.2-0.4% | ||
Copper-phosphorus Alloy Modifier CHT-TL | 0.4-0.5% | 750-760ºC | |
Phosphorus-silicate complex Modifier CHT-BZ1 | 0.8-1.2& | ||
Phosphorus-sulfur complex Modifier CHT-BZ2 | 1.2-1.5% | ||
Three-component Modifier CHT-BZ3 | 2-3% | ||
Refining Modifier CHT-BZ4 | 1.4-1.6% | ||
Strontium Slat long-seffect Modifier CHT-BZ5 | 1.0% | >720ºC |