| Alloy or Not: | Alloy |
|---|---|
| Standard: | ISO9001 |
| Transport Package: | in Bundles Wrapped Plastic Film and Strapped on PA |

Application:
It is widely applicable to new type of advanced material and special alloys
Main products of the chemical composition:
Metal fluxer series:
| Name | Usage% | Temperature/ºC | Use |
| Coverer CHT-FG | 0.8-0.1kg/m2 | <660ºC | All other kinds of aluminium and aluminium alloy except high magnesium alloy. |
| Magnesium coverer CHT-MF | 0.5-1.0kg/m2 | 450ºC | Mainly for the covering of magnesium and magnesium alloy to avoid oxidation damage |
| Sodium -free coverer CHT-WNF | 0.3kg/m2 | 700-740ºC | For the covering of aluminium melt that cannot touch sodium to avoid oxidizing and damaging the aluminium liquid. |
| Fluxer 1 CHT-JL1 | 0.3<0.5% | 640ºC | Used for refining of series of processing aluminium alloy and pure aluminium except for high magnesium and popularly. |
| Magnesium Refiner CHT-MJ | 1-1.5kg/Tm | 450ºC | Mainly for the degassing and slag removal of magnesium and magnesium alloy |
| Degassing refiner CHT-CJL | 0.1-0.2% | 680-750ºC | Degassing refiner is a relatively traditional lump refiner; it has a double effect of slag removal and degassing. By far, it is widely acknowledged as the most effective solid refiner. |
| High-efficiency and Non-toxic Refiner CHT-GJL | 0.1-0.2% | 680ºC | For aluminium and aluminium alloy except high magnesium ally |
| Sodium-free Refiner CHT-WNJ | 2-5 kg/T al | 700-730ºC | The product mainly for the aluminium alloy, degassing and slag removal of wheel hubs, pistons and sodium of cars. |
| Power spraying refiner CHT-PJL | 0.1-0.2% | 700-750ºC | It has the product mainly |
| Universal Fluxer CHT-WN | 0.2-0.5% | 710-750ºC | |
| Phosphorus-copper Modifier CHT-LT | 0.4-0.6% | ||
| Aluminium-phosphorus Alloy Modifier CHT-LL | 0.2-0.4% | ||
| Copper-phosphorus Alloy Modifier CHT-TL | 0.4-0.5% | 750-760ºC | |
| Phosphorus-silicate complex Modifier CHT-BZ1 | 0.8-1.2& | ||
| Phosphorus-sulfur complex Modifier CHT-BZ2 | 1.2-1.5% | ||
| Three-component Modifier CHT-BZ3 | 2-3% | ||
| Refining Modifier CHT-BZ4 | 1.4-1.6% | ||
| Strontium Slat long-seffect Modifier CHT-BZ5 | 1.0% | >720ºC |

FAQ: